HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene
Empreu sempre aquest identificador per citar o enllaçar aquest ítem
http://hdl.handle.net/10045/2299
Títol: | HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene |
---|---|
Autors: | Marcilla, Antonio | Beltrán, Maribel | Hernández, F. | Navarro Martínez, Rosa María |
Grups d'investigació o GITE: | Procesado y Pirólisis de Polímeros |
Centre, Departament o Servei: | Universidad de Alicante. Departamento de Ingeniería Química |
Paraules clau: | Catalytic pyrolysis | Catalyst activity | Deactivation | Coke deposition | HZSM5 | HUSY | HDPE | LDPE |
Àrees de coneixement: | Ingeniería Química |
Data de publicació: | 28-de desembre-2004 |
Editor: | Elsevier |
Citació bibliogràfica: | MARCILLA GOMIS, Antonio, et al. "HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene". Applied Catalysis A: General. Vol. 278, Issue 1 (28 Dec. 2004). ISSN 0926-860X, pp. 37-43 |
Resum: | Se estudia el proceso de desactivación de los catalizadores HZSM5 y HUSY durante la pirólisis catalítica de LDPE y HDPE. Para explicar el comportamiento encontrado en cada caso debe considerarse no sólo las propiedades texturales de la zeolita, sino también su acidez así como la estructura del polímero. | The behaviour of HZSM5 and HUSY zeolites during the decomposition of low density (LDPE) and high density polyethylene (HDPE) has been studied by TGA. Zeolites have been thoroughly characterized in order to elucidate the structures responsible for the observed behaviour. The reduction in the decomposition temperature is initially very high with HUSY for both polyethylenes while for HZSM5 is much greater with the branched LDPE than with linear HDPE. To explain the relative activity of these zeolites and the differences found for HZSM5 with both polyethylenes the polymer structure, the zeolite acidity and its textural properties have to be considered. The progressive deactivation behaviour of the catalysts has also been studied. HUSY shows a fast deactivation while small pore size in HZSM5 prevents coke deposition. Completely deactivated zeolites still show a considerable number of apparently unaltered acid sites. |
Patrocinadors: | Comisión de Investigación de Ciencia y Tecnología de la Secretaría de Estado de Educación, Universidades, Investigación y Desarrollo, CICYT (PQ2001-073), la Comunidad Europea (Fondos FEDER) y la Generalitat Valenciana (GV01-42) |
URI: | http://hdl.handle.net/10045/2299 |
ISSN: | 0926-860X |
DOI: | 10.1016/j.apcata.2004.09.023 |
Idioma: | eng |
Tipus: | info:eu-repo/semantics/article |
Revisió científica: | si |
Versió de l'editor: | http://dx.doi.org/10.1016/j.apcata.2004.09.023 |
Apareix a la col·lecció: | INV - GTP3 - Artículos de Investigación sobre Pirólisis Catalítica de Polímeros |
Arxius per aquest ítem:
Arxiu | Descripció | Tamany | Format | |
---|---|---|---|---|
HZSM5 and HUSY deactivation.pdf | Versión final (acceso restringido) | 382,2 kB | Adobe PDF | Obrir Sol·licitar una còpia |
Tots els documents dipositats a RUA estan protegits per drets d'autors. Alguns drets reservats.