HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene

Please use this identifier to cite or link to this item: http://hdl.handle.net/10045/2299
Información del item - Informació de l'item - Item information
Title: HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene
Authors: Marcilla, Antonio | Beltrán, Maribel | Hernández, F. | Navarro Martínez, Rosa María
Research Group/s: Procesado y Pirólisis de Polímeros
Center, Department or Service: Universidad de Alicante. Departamento de Ingeniería Química
Keywords: Catalytic pyrolysis | Catalyst activity | Deactivation | Coke deposition | HZSM5 | HUSY | HDPE | LDPE
Knowledge Area: Ingeniería Química
Issue Date: 28-Dec-2004
Publisher: Elsevier
Citation: MARCILLA GOMIS, Antonio, et al. "HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene". Applied Catalysis A: General. Vol. 278, Issue 1 (28 Dec. 2004). ISSN 0926-860X, pp. 37-43
Abstract: Se estudia el proceso de desactivación de los catalizadores HZSM5 y HUSY durante la pirólisis catalítica de LDPE y HDPE. Para explicar el comportamiento encontrado en cada caso debe considerarse no sólo las propiedades texturales de la zeolita, sino también su acidez así como la estructura del polímero. | The behaviour of HZSM5 and HUSY zeolites during the decomposition of low density (LDPE) and high density polyethylene (HDPE) has been studied by TGA. Zeolites have been thoroughly characterized in order to elucidate the structures responsible for the observed behaviour. The reduction in the decomposition temperature is initially very high with HUSY for both polyethylenes while for HZSM5 is much greater with the branched LDPE than with linear HDPE. To explain the relative activity of these zeolites and the differences found for HZSM5 with both polyethylenes the polymer structure, the zeolite acidity and its textural properties have to be considered. The progressive deactivation behaviour of the catalysts has also been studied. HUSY shows a fast deactivation while small pore size in HZSM5 prevents coke deposition. Completely deactivated zeolites still show a considerable number of apparently unaltered acid sites.
Sponsor: Comisión de Investigación de Ciencia y Tecnología de la Secretaría de Estado de Educación, Universidades, Investigación y Desarrollo, CICYT (PQ2001-073), la Comunidad Europea (Fondos FEDER) y la Generalitat Valenciana (GV01-42)
URI: http://hdl.handle.net/10045/2299
ISSN: 0926-860X
DOI: 10.1016/j.apcata.2004.09.023
Language: eng
Type: info:eu-repo/semantics/article
Peer Review: si
Publisher version: http://dx.doi.org/10.1016/j.apcata.2004.09.023
Appears in Collections:INV - GTP3 - Artículos de Investigación sobre Pirólisis Catalítica de Polímeros

Files in This Item:
Files in This Item:
File Description SizeFormat 
ThumbnailHZSM5 and HUSY deactivation.pdfVersión final (acceso restringido)382,2 kBAdobe PDFOpen    Request a copy


Items in RUA are protected by copyright, with all rights reserved, unless otherwise indicated.