New Binary Blends of Ethylene-co-n-butyl Acrylate (EBA) Copolymer and Low Molecular Weight Rosin Ester Resin with Potential as Pressure Sensitive Adhesives

Por favor, use este identificador para citar o enlazar este ítem: http://hdl.handle.net/10045/82428
Información del item - Informació de l'item - Item information
Título: New Binary Blends of Ethylene-co-n-butyl Acrylate (EBA) Copolymer and Low Molecular Weight Rosin Ester Resin with Potential as Pressure Sensitive Adhesives
Autor/es: Sancho-Querol, Sara | Yáñez-Pacios, Andrés Jesús | Martín-Martínez, José Miguel
Grupo/s de investigación o GITE: Adhesión y Adhesivos
Centro, Departamento o Servicio: Universidad de Alicante. Departamento de Química Inorgánica
Palabras clave: Ethylene-co-n-butyl acrylate copolymer | Glycerol rosin ester | Pressure sensitive adhesive | Compatibility | Tack | Adhesion
Área/s de conocimiento: Química Inorgánica
Fecha de publicación: 19-oct-2018
Editor: MDPI
Cita bibliográfica: Sancho-Querol S, Yáñez-Pacios AJ, Martín-Martínez JM. New Binary Blends of Ethylene-co-n-butyl Acrylate (EBA) Copolymer and Low Molecular Weight Rosin Ester Resin with Potential as Pressure Sensitive Adhesives. Materials. 2018; 11(10):2037. doi:10.3390/ma11102037
Resumen: For improving the adhesion property of ethylene-co-n-butyl acrylate copolymer (EBA) at ambient temperature, binary blends of EBA with 27 wt% n-butyl acrylate and different amounts (20–62 wt%) of low molecular weight hydrogenated glycerol rosin ester (ECH) resin have been prepared. The addition of glycerol rosin ester resin decreased the crystallinity and size of the ethylene domains of the EBA copolymer. The addition of up to 50 wt% (100 phr) ECH resin improved the compatibility with the EBA copolymer, whereas when more than 50 wt% (100 phr) ECH resin was added, the compatibility of the blends did not change but the viscoelastic properties were noticeably decreased. Furthermore, the compatibility was noticeably improved by adding only 20 wt% ECH resin although the best compromise between compatibility and viscoelasticity corresponded to the binary blend made with 43 wt% ECH resin. The EBA copolymer + ECH resin blends showed high tack (initial adhesion) at 25 °C and some of them even at 5 °C, and they have adequate 180° peel strength both to polar (polyethylene terephthalate-PET) and nonpolar (polypropylene-PP) substrate. Furthermore, all EBA copolymer + ECH resin blends showed high shear strength at 25 °C. Finally, the blend with 43 wt% ECH resin showed excellent pressure sensitive adhesive property exhibiting excellent creep, high tack, high 180° peel strength, and high single lap-shear strength.
URI: http://hdl.handle.net/10045/82428
ISSN: 1996-1944
DOI: 10.3390/ma11102037
Idioma: eng
Tipo: info:eu-repo/semantics/article
Derechos: © 2018 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (http://creativecommons.org/licenses/by/4.0/).
Revisión científica: si
Versión del editor: https://doi.org/10.3390/ma11102037
Aparece en las colecciones:INV - LAA - Artículos de Revistas

Archivos en este ítem:
Archivos en este ítem:
Archivo Descripción TamañoFormato 
Thumbnail2018_Sancho-Querol_etal_Materials.pdf6,54 MBAdobe PDFAbrir Vista previa


Este ítem está licenciado bajo Licencia Creative Commons Creative Commons