HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene
Por favor, use este identificador para citar o enlazar este ítem:
http://hdl.handle.net/10045/2299
Título: | HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene |
---|---|
Autor/es: | Marcilla, Antonio | Beltrán, Maribel | Hernández, F. | Navarro Martínez, Rosa María |
Grupo/s de investigación o GITE: | Procesado y Pirólisis de Polímeros |
Centro, Departamento o Servicio: | Universidad de Alicante. Departamento de Ingeniería Química |
Palabras clave: | Catalytic pyrolysis | Catalyst activity | Deactivation | Coke deposition | HZSM5 | HUSY | HDPE | LDPE |
Área/s de conocimiento: | Ingeniería Química |
Fecha de publicación: | 28-dic-2004 |
Editor: | Elsevier |
Cita bibliográfica: | MARCILLA GOMIS, Antonio, et al. "HZSM5 and HUSY deactivation during the catalytic pyrolysis of polyethylene". Applied Catalysis A: General. Vol. 278, Issue 1 (28 Dec. 2004). ISSN 0926-860X, pp. 37-43 |
Resumen: | Se estudia el proceso de desactivación de los catalizadores HZSM5 y HUSY durante la pirólisis catalítica de LDPE y HDPE. Para explicar el comportamiento encontrado en cada caso debe considerarse no sólo las propiedades texturales de la zeolita, sino también su acidez así como la estructura del polímero. | The behaviour of HZSM5 and HUSY zeolites during the decomposition of low density (LDPE) and high density polyethylene (HDPE) has been studied by TGA. Zeolites have been thoroughly characterized in order to elucidate the structures responsible for the observed behaviour. The reduction in the decomposition temperature is initially very high with HUSY for both polyethylenes while for HZSM5 is much greater with the branched LDPE than with linear HDPE. To explain the relative activity of these zeolites and the differences found for HZSM5 with both polyethylenes the polymer structure, the zeolite acidity and its textural properties have to be considered. The progressive deactivation behaviour of the catalysts has also been studied. HUSY shows a fast deactivation while small pore size in HZSM5 prevents coke deposition. Completely deactivated zeolites still show a considerable number of apparently unaltered acid sites. |
Patrocinador/es: | Comisión de Investigación de Ciencia y Tecnología de la Secretaría de Estado de Educación, Universidades, Investigación y Desarrollo, CICYT (PQ2001-073), la Comunidad Europea (Fondos FEDER) y la Generalitat Valenciana (GV01-42) |
URI: | http://hdl.handle.net/10045/2299 |
ISSN: | 0926-860X |
DOI: | 10.1016/j.apcata.2004.09.023 |
Idioma: | eng |
Tipo: | info:eu-repo/semantics/article |
Revisión científica: | si |
Versión del editor: | http://dx.doi.org/10.1016/j.apcata.2004.09.023 |
Aparece en las colecciones: | INV - GTP3 - Artículos de Investigación sobre Pirólisis Catalítica de Polímeros |
Archivos en este ítem:
Archivo | Descripción | Tamaño | Formato | |
---|---|---|---|---|
HZSM5 and HUSY deactivation.pdf | Versión final (acceso restringido) | 382,2 kB | Adobe PDF | Abrir Solicitar una copia |
Todos los documentos en RUA están protegidos por derechos de autor. Algunos derechos reservados.